Paint is a very common item in home decoration, even in the industry there are "three points woodworking seven points paint" said. The position of the paint process in the renovation is critical. The author's commonly used paint process sequence is listed below for your reference.
Dulux (good mood) Yuting furniture
〠一ã€Wood lacquer 】
1, varnish process
1) Coloring oil or coloring oil (Note: Only for projects that require discoloration, this process is not required for ordinary projects.)
2) Brushing varnish protection primer (if there is no first step process, this is the first process)
If it is to maintain the original color for varnishing, then the surface must be cleaned and the first pass of the protective primer must be carried out immediately after the material is purchased in the construction site. Primers are also generally topcoats. * Varnish finish painting must be done before wall paint is applied.
3) Clean the wood surface of dust and dirt.
4) Polish the surface of the board or wood with sandpaper.
5) Brush the paint the first time.
6) After drying out, use the formulated toner, cooked rubber powder, and fly powder to adjust the putty to cover off the nails and tree shrews so that they are the same as their natural colors.
7) After dry, polish the rough part of the toner with fine sandpaper. This is a critical step. Be sure to light the surface.
8) Brush paint again.
9) Dry sandpaper after polishing
10) Brush the paint again (i.e. paint it again with fine sandpaper, and so on. If there is a special primer, change the first coat to a special primer).
11) Wet the cloth first to wet the surface of the wood, then wet the surface with sandpaper, then polish the surface, commonly known as water mill.
12) Brush the last time the paint. In general, when you count the last lacquer, a total of about 4 to 8 passes will be required to achieve a better quality. The more surface paints the better, but generally not more than 10 times.
In the wet weather construction, the paint film will be whitish. The addition of nitromagnetized white water with a diluent amount of 10~15% can eliminate it.
2, mixed oil process
1) Clean up the dust and dirt on the surface of the wood.
2) Mix the surface of the batch of woodware with pig blood plus fly powder.
3) Dry with sandpaper
4) Brush the first time
5) Make up for bad points.
6) Dry with sandpaper
7) Brush the second time
8) Dry with sandpaper
9) Brush the paint three times.
In general, it is advisable to mix oil two to three times.
Experience on the wall construction paint project interior decoration latex paint home furniture panel furniture decoration home
Resin bond is a kind of organic bond, the grinding wheel made of this bond has high strength, has certain elasticity, low heat resistance, good self-sharpening, easy production and short process cycle. It can manufacture Grinding Wheels with working speed higher than 50 m/s and very thin grinding wheels. Its application range is second only to ceramic binder, widely used in rough grinding, waste grinding, cutting and free grinding, such as grinding steel ingot, casting burr etc.. Can manufacture high speed, high finish grinding wheel, heavy load, cutting and various special requirements of grinding wheel.
In tool grinding, the cutting tool materials with high hardness, thermal hardness, wear resistance and enough strength and toughness, such as carbon tool steel, alloy tool steel, high speed steel, hard alloy, etc., are grinded with resin strong grinding wheel to achieve ideal accuracy. The surface roughness and correct geometry make the cutting edge have high sharpness and durability
Saw Blade,Brazing Diamond Saw Blade,Diamond Key Chain Saw Blade,Abrasive Paper Grinding Sheet
Henan Kemei Abrasives Co.,LTD , https://www.grindingwheelsmanufacturer.com